This paper is published in Volume-5, Issue-2, 2019
Area
Production
Author
Wasim Ahmad, Anil Verma, Priyanka Jhavar
Org/Univ
Sri Satya Sai University of Technology and Medical Sciences, Sehore, Madhya Pradesh, India
Keywords
Total Quality Management, Six Sigma, DMAIC
Citations
IEEE
Wasim Ahmad, Anil Verma, Priyanka Jhavar. A review on casting defects reduction in a foundry shop using DMAIC technique, International Journal of Advance Research, Ideas and Innovations in Technology, www.IJARIIT.com.
APA
Wasim Ahmad, Anil Verma, Priyanka Jhavar (2019). A review on casting defects reduction in a foundry shop using DMAIC technique. International Journal of Advance Research, Ideas and Innovations in Technology, 5(2) www.IJARIIT.com.
MLA
Wasim Ahmad, Anil Verma, Priyanka Jhavar. "A review on casting defects reduction in a foundry shop using DMAIC technique." International Journal of Advance Research, Ideas and Innovations in Technology 5.2 (2019). www.IJARIIT.com.
Wasim Ahmad, Anil Verma, Priyanka Jhavar. A review on casting defects reduction in a foundry shop using DMAIC technique, International Journal of Advance Research, Ideas and Innovations in Technology, www.IJARIIT.com.
APA
Wasim Ahmad, Anil Verma, Priyanka Jhavar (2019). A review on casting defects reduction in a foundry shop using DMAIC technique. International Journal of Advance Research, Ideas and Innovations in Technology, 5(2) www.IJARIIT.com.
MLA
Wasim Ahmad, Anil Verma, Priyanka Jhavar. "A review on casting defects reduction in a foundry shop using DMAIC technique." International Journal of Advance Research, Ideas and Innovations in Technology 5.2 (2019). www.IJARIIT.com.
Abstract
To become globally compatible and to gain business as well operational excellence industries are implementing various quality improvement initiatives like Lean manufacturing, ISO certification, Total Quality Management, Quality Circle, etc.. But results explored by these initiatives are time constrained and not that much profitable. So methodology, which can provide breakthrough improvement in a short time, is required to be introduced and implemented. Six Sigma is the same methodology which can provide breakthrough improvements in a short time period, so it is very essential to explore its application for gaining quantum gains and profit in terms of quality, market share and customer satisfaction.